Ti6Al4V-AlTiN涂层材料的急性毒性试验*◆

朱维东1,朱 涛1,王旭东2,蒋耀光3 【摘 要】摘要

【期刊名称】中国组织工程研究 【年(卷),期】2010(014)025 【总页数】3

【关键词】急性毒性试验;AlTiN涂层;Ti6Al4V合金;高度离子化脉冲工艺;小鼠

Supported by:Guizhou Provincial Science and Technology Project,No. 20082004*

BACKGROUND: AlTiN ceramic coatings have many advantages such as high hardness, excellent wear properties, good chemical inertness and strong adhesion, which are all consistent with the characteristics of bio-ceramics. To achieve the clinical safety, a comprehensive evaluation of acute toxicity AlTiN coating is needed.

OBJECTIVE: To test acute toxicity of Ti6Al4V-AlTiN coating materials, and to provide a reference for long-term toxicity and other toxicological tests.

METHODS: The mouse left and right femoral quadriceps muscle was injected with aseptic Ti6Al4V-AlTiN coating material, the general condition and reaction on the injection site of animals were observed at 14 days after injection, normal saline served as the negative control.

Ti6Al4V-AlTiN涂层材料的急性毒性试验

Ti6Al4V-AlTiN涂层材料的急性毒性试验*◆朱维东1,朱涛1,王旭东2,蒋耀光3【摘要】摘要【期刊名称】中国组织工程研究【年(卷),期】2010(014)025【总页数】3【关键词】急性毒性试验;AlTiN涂层;Ti6Al4V合金;高度离子化脉冲工艺;小鼠Supportedby:
推荐度:
点击下载文档文档为doc格式
47gng7ucrg6cyp27lz4y3h0qq02udc01byu
领取福利

微信扫码领取福利

微信扫码分享